STUDI EKSPERIMEN KOMBINASI PARAMETER PROSES LEACHING DENGAN DEEP EUTECTIC SOLVENT-GLYCELINE PADA RECOVERY LOGAM EMAS LIMBAH ELEKTRONIK

Khosfirah, Farah (2025) STUDI EKSPERIMEN KOMBINASI PARAMETER PROSES LEACHING DENGAN DEEP EUTECTIC SOLVENT-GLYCELINE PADA RECOVERY LOGAM EMAS LIMBAH ELEKTRONIK. Masters thesis, Institut Teknologi Sepuluh Nopember.

[thumbnail of 6007231028-MASTER_THESIS.pdf] Text
6007231028-MASTER_THESIS.pdf - Accepted Version
Restricted to Repository staff only

Download (5MB) | Request a copy

Abstract

Random Access Memory (RAM) adalah salah satu limbah komponen alat elektronik yang banyak ditemukan. Komponen alat elektronik menggunakan beberapa logam mulia sebagai pelapis, salah satunya emas (Au). Pemanfaatan limbah elektronik yang masih menggunakan cara konvensional dengan bahan kimia berbahaya dan dapat menimbulkan masalah kesehatan. Untuk itu diperlukan proses ektraksi yang lebih ramah lingkungan yaitu DES (Deep Eutectic Solvent), pelarut yang dibuat dengan mencampur HBD (Hidrogen Bond Donor) dan HBA (Hidrogen Bond Acceptor) dalam rasio molar tertentu. Penelitian ini bertujuan untuk mengevaluasi keefektifan Glyceline (DES) yang tersusun dari pencampuran Glycerol sebagai HBD dan Choline Chloride sebagai HBA dalam mengekstraksi emas (Au) dari E-Waste yang merupakan limbah Random Access Memory (RAM).
Metode penelitian yang digunakan adalah Design of Experiment Taguchi orthogonal array L9 dengan memvariasikan faktor-faktor sebagai berikut molar ratio dari Choline Chloride dibanding Glycerol (1:1, 1:1,5, dan 1:2), mass percent E-Waste (10%, 15%, dan 20%), dan stirring speed (400, 500, dan 600 rpm). Tahapan dalam proses leaching untuk mendapatkan logam emas dengan DES ini meliputi penghalusan E-Waste dengan grinder, pembuatan larutan DES, proses Leaching serbuk E-Waste dalam DES, filtrasi, pengendapan, dan recovery dengan cara membakar endapan. Pengujian dalam penelitian ini adalah X-Ray Diffraction (XRD) dan FTIR dilakukan untuk serbuk E-Waste sebelum dan sesudah Leaching, AAS untuk mengecek konsentrasi Au terlarut dalam DES, ICP-MS untuk mengecek Au yang tidak terlarut dalam DES, dan Scanning Electron Microscope (SEM) untuk mengobservasi kristal emas dari hasil recovery.
Hasil penelitian menunjukkan bahwa DES-Glyceline dengan kombinasi parameter molar ratio Choline Chloride dibanding Glycerol sebesar 1:1,5, stirring speed 600 rpm, dan konsentrasi E-Waste 15% merupakan formulasi terbaik dalam proses leaching emas. Hal tersebut berdasarkan hasil uji AAS yang menunjukkan konsentrasi emas tertinggi sebesar 0,1429 ppm, serta hasil ICP-MS menunjukkan efisiensi pelarutan emas sebesar 55,88%. Hasil uji SEM mengkonfirmasi adanya kristal emas berbentuk FCC.
====================================================================================================================================
Random Access Memory (RAM) is one of the most commonly found electronic waste components. Electronic components use several precious metals as coatings, one of which is gold (Au). The utilization of electronic waste using conventional methods with hazardous chemicals can pose health risks. Therefore, an environmentally friendly extraction process is needed, namely DES (Deep Eutectic Solvent), a solvent created by mixing HBD (Hydrogen Bond Donor) and HBA (Hydrogen Bond Acceptor) in a specific molar ratio. This study aims to evaluate the effectiveness of Glyceline (DES), composed of a mixture of Glycerol as HBD and Choline Chloride as HBA, in extracting gold (Au) from E-Waste, which is Random Access Memory (RAM) waste.
The research method used was a Design of Experiment Taguchi orthogonal array L9 with the following varying factors: molar ratio of Choline Chloride to Glycerol (1:1, 1:1.5, and 1:2), mass percent of E-Waste (10%, 15%, and 20%), and stirring speed (400, 500, and 600 rpm). The steps in the leaching process to obtain gold metal with DES include grinding E-Waste with a grinder, preparing the DES solution, leaching E-Waste powder in DES, filtration, precipitation, and recovery by burning the precipitate. The tests conducted in this study were X-Ray Diffraction (XRD) and FTIR for E-Waste powder before and after leaching, AAS to check the concentration of dissolved Au in DES, ICP-MS to check the undissolved Au in DES, and Scanning Electron Microscope (SEM) to observe the gold crystals from the recovery results.
The results of the study indicate that DES-Glycerol with a molar ratio of Choline Chloride to Glycerol of 1:1.5, stirring speed of 600 rpm, and E-Waste concentration of 15% is the optimal formulation for the gold leaching process. This is based on AAS test results showing the highest gold concentration of 0.1429 ppm, and ICP-MS results indicating gold dissolution efficiency of 55.88%. SEM test results confirmed the presence of FCC-shaped gold crystals.

Item Type: Thesis (Masters)
Uncontrolled Keywords: Recovery, E-Waste, Deep Eutectic Solvent, Choline Chloride, Glycerol
Subjects: T Technology > TP Chemical technology > TP156 Crystallization. Extraction (Chemistry). Fermentation. Distillation. Emulsions.
T Technology > TS Manufactures > TS161 Materials management.
Divisions: Faculty of Industrial Technology and Systems Engineering (INDSYS) > Mechanical Engineering > 21101-(S2) Master Thesis
Depositing User: Farah Khosfirah
Date Deposited: 04 Aug 2025 02:54
Last Modified: 04 Aug 2025 02:54
URI: http://repository.its.ac.id/id/eprint/126122